Light Weigjt Body Filler for Chevolet Mf700

Light Weigjt Body Filler for Chevolet Mf700

Application:  Acura ( Tsx(china)) Acura ( ...

OEM No/Model:  Mf700

Market Type:  After Market

Packing:  2kg 4Kg

Samples:  Free

Delivery Time:  15day

Place of origin:  China

Applicationt: 

Acura ( Tsx(china))
Acura ( Tl(china), Rsx(china), Rl(china), Mdx Trims(china), Mdx, Rl, Tl)
Aston Martin ( Db9)
Changfeng ( Liebao(china))
Chevolet ( Sail(china), Epica(china), Aveo(china), Lova Spark(china))
Daewoo ( Matiz, Rezzo, Lanos)
Fiat ( Siena(china), Weekend(china), Palio(china), Peria(china), Linea, Grand Punto, Bravo)
Ford ( S-max(china), Mondeo(china), Focus(china), Diplomat, Maverick, Edge)
Honda ( Odyssey(china), City(china), Fit(china), Accord(china), Cr-v(china), Civic(china), Stream, Fcx)
Hyundai ( Rohens, Veracruz, Equus, Azera, New Coupe, New Santa Ve)
Jeep ( Cherokee, Commander, Compass, Jeepster)

Production Description:

700 production description (Polyester Lightweight Filler)
Application& Characteristic
Quantum Premium Lightweight Filler is unsurpassed sanding qualities are the result of Quantum's patent-pending 100:1 hybrid polyester technology that utilizes an epoxy-enriched BPO catalyst.
Scope of construction: Lightweight filler is fit for ironsteel aluminumgalvanized sheet and Fiberglass.
Main performance indexes:


Item
indexes     Test method
Flexibility(mm) 50 GB/T1748
Impact strength(kg.cm) 15 GB/T1732
Thermal resistance(1h baking under 120centigrade) No bubble, no crack GB/T1735
Adhesion First class Bending method
proportion 1.0 GB/T6750
Sanding property Easy sanding Hand feel
 
 
 
 
Application:
1.Remove the oil and rust, original paint film and water etc from surface completely, keep the painted surface clean & dry before scraping.
2.The putty may cause uneven in the process of storage, must use clean ruler stir well before the use.
3The filler and BPO are mixed completely to achieve the uniformity of color (general ratio is 100:2 by weight), and apply the mixture within potlife(1-3min), or it will gel.
4Filler mixtured to the processed surface of primer or cold-reduced sheet, in case of scraping of thick coat, it is preferable to apply in thin coats for several times till reaching the objective thickness.
5Sanding should be made after hardened thoroughly. The best dry milling time is 30min after applying putty, (The temperature is 25centigrade, humidity islessthan 40%). Ensure the putty has been completely dry when painting, lest drop off or bubbles.
 
Notices:
1There is air bubble while applying, fully scrape to evenness with spatula to ensure good adhesion.
2Filler mixed with BPO recycle into garbage disposal.The filler can not lay in the air , lest volatilization &deterioration of solvent. Prohibition mixed thinner(Tianna water ) into putty.
3.When there is low temperature or high relative humidity, curing time of coating will be extended somewhat. The corresponding adjustment can be made to the consistency and gel time of putty according to the customers request.
4Our product matches with various primers, but not in phenolic primers and alkyd primers, lest drop off or bubbles. Make sure filler has been completed drying while applying putty, or cause drop off.
5The putty has special hardener is BPOcan not used with up other hardener.
6The shelf life can be up to 12 months at the cool place (under 25centigrade).