APPEARANCE: transparent, gel PROBLEM: Oxide scale and heat tint of the stainless steel surface.
GOAL: mainly for the cleaning of oxide scale and heat tint and making passivation treatment to improve the appearance and corrosion resistant ability. It is in conformity with standard: Q/SDP007-2001.
USED METHOD: Smear it on the surface of the welding seam with a thickness of 1-3mm. It needs 1-10 minutes to react.
The reaction time should be prolonged for a appropriate period when used under 0. When the reaction completed, clean it up with cloth or brush and rinse with water. CHARACTERS:
Pickling and passivation can be achieved simultaneously with the advantages such as: rapid reaction, thoroughly clean-up without generating of scar, high adhesivity, easy-operation and convenient watching. PACKAGE: 1kg/bottle, 18 kgs/carton